Curvature reduction for semiconductor wafers

A method for reducing curvature of a wafer having a semiconductor surface. One or more process steps are identified at which wafers exhibit the largest curvature, and/or wafer curvature that may reduce die yield. A crystal damaging process converts at least a portion of the semiconductor surface int...

Full description

Saved in:
Bibliographic Details
Main Authors Kirkpatrick, Brian K, Prins, Steven L, Jain, Amitabh
Format Patent
LanguageEnglish
Published 28.08.2012
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for reducing curvature of a wafer having a semiconductor surface. One or more process steps are identified at which wafers exhibit the largest curvature, and/or wafer curvature that may reduce die yield. A crystal damaging process converts at least a portion of the semiconductor surface into at least one amorphous surface region After or contemporaneously with the crystal damaging, the amorphous surface region is recrystallized by recrystallization annealing that anneals the wafer for a time ≦5 seconds at a temperature sufficient for recrystallization of the amorphous surface region. A subsequent photolithography step is facilitated due to the reduction in average wafer curvature provided by the recrystallization.