Metal oxide solid solution and use as oxygen storage composition and UV light shielding agent

Disclosed is a method for preparing a metal oxide solid solution in nano size. The metal oxide solid solution is prepared by reacting a reactant mixture containing water and at least two water-soluble metal compounds at 200 to 700° C. under a pressure of 180 to 550 bar in a continuous manner, wherei...

Full description

Saved in:
Bibliographic Details
Main Authors Myeong, Wan-Jae, Song, Kyu-Ho, Park, Se-Woong, Lee, Joo-Hyeong, Baik, Jin-Soo, Chung, Chang-Mo
Format Patent
LanguageEnglish
Published 20.04.2010
Online AccessGet full text

Cover

Loading…
More Information
Summary:Disclosed is a method for preparing a metal oxide solid solution in nano size. The metal oxide solid solution is prepared by reacting a reactant mixture containing water and at least two water-soluble metal compounds at 200 to 700° C. under a pressure of 180 to 550 bar in a continuous manner, wherein the reactant mixture contains the metal compounds at an amount of 0.01 to 30% by weight in total and the solid solution has a crystallite size of 1 to 1,000 nm. The metal oxide solid solution is, in particular suitable as a UV light shielding agent or as an oxygen storage component.