Wear resistant aluminum alloy elongate body, manufacturing method thereof and piston for car air conditioner

The wear resistant aluminum alloy elongate body contains 7-13 mass % of Si, 0.001-0.3 mass % of iron, 2.0-5.0 mass % of Cu, 0.3-1.0 mass % of Mg, 0.001-0.3 mass % of Mn, 0.001-0.3 mass % of Cr, 0.003-0.03 mass % of Sr, 0.005-0.05 mass % of Ti, and the remaining part of Al and unavoidable impurity. T...

Full description

Saved in:
Bibliographic Details
Main Authors Sato, Shinichi, Kato, Takayuki, Deto, Norikazu, Nojiri, Masashi, Ikeda, Toshiya, Nakai, Yoshihiro, Kishikawa, Yoshiki, Utsunomiya, Kiyotaka
Format Patent
LanguageEnglish
Published 06.02.2003
Online AccessGet full text

Cover

Loading…
More Information
Summary:The wear resistant aluminum alloy elongate body contains 7-13 mass % of Si, 0.001-0.3 mass % of iron, 2.0-5.0 mass % of Cu, 0.3-1.0 mass % of Mg, 0.001-0.3 mass % of Mn, 0.001-0.3 mass % of Cr, 0.003-0.03 mass % of Sr, 0.005-0.05 mass % of Ti, and the remaining part of Al and unavoidable impurity. The size of Si grains existing in the elongate body is, by the average value, at most 10 m and by the maximum value, at most 30 m, and the size of the Si grains in the range of down to 1.5 mm deep from the surface is, by the maximum value, at most 6 m. Further, crystal texture of Al alloy is one selected from the group consisting of hot rolled texture, re-crystallized texture and mixed texture of hot rolled texture and re-crystallized texture.