Stability of SiC/SiC fibre composites exposed to Li sub 4 SiO sub 4 and Li sub 2 TiO sub 3 in fusion relevant conditions
The physico-chemical stability of a commercial 3D SiC sub f /SiC composite provided with an outer CVD SiC protective layer was studied after exposure to flowing helium with 0.1% H sub 2 at 800 deg C in contact with lithium silicate and lithium titanate. Exposure tests were carried out for 216, 1000...
Saved in:
Published in | Journal of nuclear materials Vol. 294; no. 3; pp. 223 - 231 |
---|---|
Main Authors | , , , , |
Format | Journal Article |
Language | English |
Published |
01.04.2001
|
Online Access | Get full text |
Cover
Loading…
Summary: | The physico-chemical stability of a commercial 3D SiC sub f /SiC composite provided with an outer CVD SiC protective layer was studied after exposure to flowing helium with 0.1% H sub 2 at 800 deg C in contact with lithium silicate and lithium titanate. Exposure tests were carried out for 216, 1000 and 10 000 h in an especially designed loop. The mechanical characteristics of the SiC sub f /SiC composite in contact with Li sub 4 SiO sub 4 were almost unaffected by the exposure, while those in contact with Li sub 2 TiO sub 3 were slightly worsened. SiC coating transformation was clearly detected on samples exposed to both lithium silicate and titanate. Copyright (c) 2001 Elsevier Science B.V. |
---|---|
Bibliography: | ObjectType-Article-2 SourceType-Scholarly Journals-1 content type line 23 ObjectType-Feature-1 |
ISSN: | 0022-3115 |