The properties of ion-implanted LiNbO sub(3 waveguides measured by the RBS and ion beam etching stripping methods)

Z-cut LiNbO sub(3 crystals were implanted at room temperature with 3.0 MeV O ions with a fluence of 6 x 10[super]14 ions/cm[super]2. The effective refractive index of the guided mode was obtained by the prism coupling technique combined with mechanical stripping (ion beam etching) at room temperatur...

Full description

Saved in:
Bibliographic Details
Published inOptical materials Vol. 33; no. 8; pp. 1357 - 1361
Main Authors Zhao, Jin-Hua, Huang, Qing, Wang, Lei, Fu, Gang, Qin, Xi-Feng, Liu, Peng, Guo, Sha-Sha, Liu, Tao, Wang, Xue-Lin
Format Journal Article
LanguageEnglish
Published 01.06.2011
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Z-cut LiNbO sub(3 crystals were implanted at room temperature with 3.0 MeV O ions with a fluence of 6 x 10[super]14 ions/cm[super]2. The effective refractive index of the guided mode was obtained by the prism coupling technique combined with mechanical stripping (ion beam etching) at room temperature. Surface layers, with thicknesses of 300, 630, 880, 1100, and 1500 nm, were removed. The channel spectra of LiNbO) sub(3) waveguides with different etching depths were measured by the RBS technique. The damage profile of the LiNbO sub(3 waveguide was studied by dechannelling analysis with a multiple scattering function based on the channel spectrum. The refractive index profile was calculated based on the lattice damage ratio. The effective refractive index of the guided mode simulated by BPM showed good agreement with the experiment value.)
Bibliography:ObjectType-Article-1
SourceType-Scholarly Journals-1
content type line 23
ObjectType-Feature-2
ISSN:0925-3467
DOI:10.1016/j.optmat.2011.03.043