Interaction of sintered aluminum nitride with the KF-AlF^sub 3^ melt at 700-800°C

Interaction kinetics of the aluminum nitride-based sintered composite material with the potassium cryolite melt with the cryolite ratio KO = 1.3 at 700-800°C is investigated by the continuous weighing method. It is established that the composite is almost unaffected by the melt at t = 700°C. The cor...

Full description

Saved in:
Bibliographic Details
Published inRussian journal of non-ferrous metals Vol. 55; no. 5; p. 419
Main Authors Chuikin, A Yu, Zaikov, Yu P, Beketov, A R
Format Journal Article
LanguageEnglish
Published New York Springer Nature B.V 01.09.2014
Online AccessGet full text

Cover

Loading…
More Information
Summary:Interaction kinetics of the aluminum nitride-based sintered composite material with the potassium cryolite melt with the cryolite ratio KO = 1.3 at 700-800°C is investigated by the continuous weighing method. It is established that the composite is almost unaffected by the melt at t = 700°C. The corrosion rate increases as the temperature increases. The material interacts with the molten salt through its oxidation stage by oxygen dissolved in the melt. This is also accompanied by the dissolution of oxygen-containing impurities that are initially present in the material. No interaction of sintered aluminum nitride with the melt under study was observed in the absence of the oxidant and with the concentration of alumina dissolved in cryolite close to saturation.[PUBLICATION ABSTRACT]