Al-Si-Cu계 AC2B 합금의 최적 용체화 처리 조건
The precipitates, hardness, and tensile properties of Al-6.2Si-2.9Cu AC2B alloy were investigated with respect to solution treatment time at 500˚C. Al(Cu)-Al2Cu eutectic, Si, θ-(Al2Cu), and Q-(Al5Cu2Mg8Si6) phases were observed in the as-cast specimen. With increasing the solution treatment time at...
Saved in:
Published in | 대한금속·재료학회지, 47(4) pp. 223 - 227 |
---|---|
Main Authors | , , , , , , |
Format | Journal Article |
Language | Korean |
Published |
대한금속·재료학회
01.05.2009
|
Subjects | |
Online Access | Get full text |
ISSN | 1738-8228 2288-8241 |
Cover
Summary: | The precipitates, hardness, and tensile properties of Al-6.2Si-2.9Cu AC2B alloy were investigated
with respect to solution treatment time at 500˚C. Al(Cu)-Al2Cu eutectic, Si, θ-(Al2Cu), and Q-(Al5Cu2Mg8Si6)
phases were observed in the as-cast specimen. With increasing the solution treatment time at 500˚C, the
Al(Cu)-Al2Cu eutectic and θ-(Al2Cu) phases were gradually reduced and finally almost disappeared in 5 h. The
mechanical properties, such as hardness, tensile strength, and elongation, were improved with solution
treatment time until about 5 h due to the dissolution of the Al2Cu particles. With further holding time, the
mechanical properties did not change much. The solution treated specimens for over 5 h at 500˚
C exhibit
almost the same tensile properties even after aging at 250˚C for 3.5 h. Accordingly, the optimal solution
treatment condition of the Al-Si-Cu AC2B alloy is considered to be 5 h at 500˚C. KCI Citation Count: 8 |
---|---|