COPOLYESTERS,PREPARATION AND USE THEREOF

Water-soluble polyester having an apparent molecular weight between about 600 and about 5,000 and a SO3M group content between about 5 to about 40 mol percent based on the number of mols of dicarboxylic and/or polycarboxylic acids esterified in the polyester, and an at least trifunctional alcohol an...

Full description

Saved in:
Bibliographic Details
Main Authors BEUTLER H, ENGELHARDT F, RIBKA J, HINTERMEIER K
Format Patent
LanguageEnglish
Published 26.04.1978
Edition2
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Water-soluble polyester having an apparent molecular weight between about 600 and about 5,000 and a SO3M group content between about 5 to about 40 mol percent based on the number of mols of dicarboxylic and/or polycarboxylic acids esterified in the polyester, and an at least trifunctional alcohol and/or an at least trifunctional carboxylic acid content between about 1 to about 40 mol percent based on the number of mols of dicarboxylic and/or polycarboxylic acids esterified in the polyester so that the polyester is correspondingly branched and M denotes a cation of an alkali metal, the ammonium ion or the cationic radical of an organic amine. The improved polyester is particularly suited as a levelling agent in the disperse dyeing of polyester fibers or the like.
Bibliography:Application Number: ZA19770002866