Catalyst manufacture

A method is described for lowering the nitrate content in a cobalt catalyst precursor formed by impregnating a catalyst support with cobalt nitrate, comprising calcining the impregnated support in air to effect partial denitrification and subsequently heating the calcined impregnated support to a te...

Full description

Saved in:
Bibliographic Details
Main Authors ANTONINI, ALEJANDRO MARTIN, CASCI, JOHN LEONELLO
Format Patent
LanguageEnglish
Published 26.11.2008
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method is described for lowering the nitrate content in a cobalt catalyst precursor formed by impregnating a catalyst support with cobalt nitrate, comprising calcining the impregnated support in air to effect partial denitrification and subsequently heating the calcined impregnated support to a temperature below 250° C. in the presence of a gas mixture comprising 0.1-10% hydrogen by volume in an inert gas.
Bibliography:Application Number: ZA20070009451