PITCH COMPOSITIONS FOR SPINNING INTO CARBON ARTICLES AND METHODS RELATING THERETO

A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (Tsp) of 400°C or less, and an oxidation onset temperature (OOT) at least 10°C below the Tsp at a ramp rate of 10°C/min. A carbon fiber may comprise: a carbon fiber produced from a pitch composition,...

Full description

Saved in:
Bibliographic Details
Main Authors SMITH, Stuart E, PANEPINTO, Robert, CHASE, Clarence E, VADLAMUDI, Madhavi
Format Patent
LanguageEnglish
French
Published 14.07.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (Tsp) of 400°C or less, and an oxidation onset temperature (OOT) at least 10°C below the Tsp at a ramp rate of 10°C/min. A carbon fiber may comprise: a carbon fiber produced from a pitch composition, wherein the pitch composition comprises: a pitch having a softening point temperature (Tsp) of 400°C or less, and an oxidation onset temperature (OOT) at least 10°C below the Tsp at a ramp rate of 10°C/min. Une composition de brai appropriée pour le filage peut comprendre : un brai ayant une température de point de ramollissement (Tsp) inférieure ou égale à 400 °C, et une température de début d'oxydation (OOT) d'au moins 10 °C en dessous de Tsp à une vitesse de rampe de 10 °C/min. Une fibre de carbone peut comprendre : une fibre de carbone produite à partir d'une composition de brai, la composition de brai comprenant : un brai ayant une température de point de ramollissement (Tsp) inférieure ou égale à 400 °C, et une température de début d'oxydation (OOT) d'au moins 10 °C en dessous de Tsp à une vitesse de rampe de 10 °C/min.
Bibliography:Application Number: WO2021US72318