WATER-ABSORBING RESIN PARTICLES AND ABSORBENT ARTICLE
Disclosed are water-absorbing resin particles 10a constituted of polymer particles that have been surface crosslinked by a surface crosslinking agent. When the water-absorbing resin particles are allowed to absorb physiological saline solution for ten minutes under a load of 2.07 kPa, the amount of...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English French Japanese |
Published |
18.03.2021
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Disclosed are water-absorbing resin particles 10a constituted of polymer particles that have been surface crosslinked by a surface crosslinking agent. When the water-absorbing resin particles are allowed to absorb physiological saline solution for ten minutes under a load of 2.07 kPa, the amount of water absorbed per 1.00 g of water-absorbing resin particles is 5 to 35 mL/g. The ten-minute value of non-pressurized DW of the water-absorbing resin particles is 1 to 50 mL/g.
L'invention concerne des particules de résine absorbant l'eau (10a) constituées de particules de polymère qui ont été réticulées en surface par un agent de réticulation de surface. Lorsque les particules de résine absorbant l'eau sont autorisées à absorber une solution saline physiologique pendant dix minutes sous une charge de 2,07 kPa, la quantité d'eau absorbée par 1,00 g de particules de résine absorbant l'eau est de 5 à 35 mL/g. La valeur à dix minutes du DW non pressurisé des particules de résine absorbant l'eau est de 1 à 50 mL/g.
表面架橋剤によって表面架橋された重合体粒子を含む、吸水性樹脂粒子10aが開示される。吸水性樹脂粒子に2.07kPaの荷重下で生理食塩水を10分間吸収させたときの吸水性樹脂粒子1.00g当たりの吸水量が5~35mL/gである。吸水性樹脂粒子の無加圧DWの10分値が、1~50mL/gである。 |
---|---|
Bibliography: | Application Number: WO2020JP33953 |