PROCESS FOR MODIFYING LDPE
Process for obtaining polyethylene with an MFI (190°C/2.16 kg) of at least 4 g/10 minutes and a melt strength (190°C) of at least 8.0 cN, said process involving extrusion of low density polyethylene (LDPE) with an MFI of at least 5 g/10 minutes and a vinyl content of less than 0.25 terminal vinyl gr...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English French |
Published |
19.12.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Process for obtaining polyethylene with an MFI (190°C/2.16 kg) of at least 4 g/10 minutes and a melt strength (190°C) of at least 8.0 cN, said process involving extrusion of low density polyethylene (LDPE) with an MFI of at least 5 g/10 minutes and a vinyl content of less than 0.25 terminal vinyl groups per 1000 C-atoms (measured with NMR in deuterated tetrachloroethane solution) - in the presence of 500-5,000 ppm, based on the weight of low density polyethylene, of an organic peroxide.
L'invention concerne un procédé d'obtention de polyéthylène ayant un indice de fluidité (MFI) (190 °C/2,16 kg) d'au moins 4 g/10 minutes et une résistance à l'état fondu (190 °C) d'au moins 8,0 cN, ledit procédé impliquant l'extrusion de polyéthylène basse densité (LDPE) avec un MFI d'au moins 5 g/10 minutes et une teneur en vinyle inférieure à 0,25 groupe vinyle terminal pour 00 atome de C (mesuré par RMN dans une solution de tétrachloroéthane deutéré) en présence de 500 à 5 000 ppm, par rapport au poids de polyéthylène basse densité, d'un peroxyde organique. |
---|---|
Bibliography: | Application Number: WO2018EP82319 |