INFRARED STEALTH COATING AND PREPARATION METHOD THEREFOR
An infrared stealth coating and a preparation method therefor. The infrared stealth coating comprises, in weight percent: 40.0 to 50.0% of an organosilicone resin, 1.0 to 40.0% of a filler, 10.0 to 20.0% of a pigment, 0.5 to 5.0% of a dispersant, 0.2 to 1.5% of a wetting agent, 0.5 to 5.0% of a thic...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | Chinese English French |
Published |
04.04.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | An infrared stealth coating and a preparation method therefor. The infrared stealth coating comprises, in weight percent: 40.0 to 50.0% of an organosilicone resin, 1.0 to 40.0% of a filler, 10.0 to 20.0% of a pigment, 0.5 to 5.0% of a dispersant, 0.2 to 1.5% of a wetting agent, 0.5 to 5.0% of a thickener, 0.0 to 1.5% of a flatting agent, 0.5 to 3.0% of a film-forming aid, 0.0 to 0.5% of a defoaming agent, and the balance of deionized water.
L'invention concerne un revêtement furtif à infrarouge et son procédé de préparation. Le revêtement furtif à infrarouge comprend, en pourcentage en poids : de 40,0 à 50,0 % d'une résine d'organosilicone, de 1,0 à 40,0 % d'une charge, de 10,0 à 20,0 % d'un pigment, de 0,5 à 5,0 % d'un agent dispersant, de 0,2 à 1,5 % d'un agent mouillant, de 0,5 à 5,0 % d'un épaississant, de 0,0 à 1,5 % d'un agent de matité, de 0,5 à 3,0 % d'un agent auxiliaire filmogène, de 0,0 à 0,5 % d'un agent antimousse, et le reste étant de l'eau désionisée.
一种红外隐身涂料及其制备方法,按重量百分比,该红外隐身涂料包括:40.0~50.0%的 |
---|---|
Bibliography: | Application Number: WO2018CN83685 |