HEAT-RESISTANT SINTERED MATERIAL HAVING EXCELLENT OXIDATION RESISTANCE, WEAR RESISTANCE AT HIGH TEMPERATURES AND SALT DAMAGE RESISTANCE, AND METHOD FOR PRODUCING SAME

This heat-resistant sintered material has a composition which contains, in mass% as a whole composition, 20-38% of Cr, 0.5-3.0% of Mo, 3.0-7.0% of Si and 0.5-2.5% of C with the balance made up of Fe and unavoidable impurities. This heat-resistant sintered material has a structure wherein hard phases...

Full description

Saved in:
Bibliographic Details
Main Authors FUKUDA Ryosuke, MIYAHARA Masahisa
Format Patent
LanguageEnglish
French
Japanese
Published 04.10.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:This heat-resistant sintered material has a composition which contains, in mass% as a whole composition, 20-38% of Cr, 0.5-3.0% of Mo, 3.0-7.0% of Si and 0.5-2.5% of C with the balance made up of Fe and unavoidable impurities. This heat-resistant sintered material has a structure wherein hard phases are dispersed in a matrix; the matrix contains Fe, Cr, Mo and Si; the hard phases contain Cr, Fe, Mo and C; and the porosity is 2.0% or less. Le matériau fritté résistant à la chaleur selon l'invention a une composition qui contient, en % en masse de la composition totale, de 20 à 38 % de Cr, de 0,5 à 3,0 % de Mo, de 3,0 à 7,0 % de Si et de 0,5 à 2,5 % de C, le reste étant constitué de Fe et d'impuretés inévitables. Ce matériau fritté résistant à la chaleur a une structure dans laquelle des phases dures sont dispersées dans une matrice ; la matrice contient Fe, Cr, Mo et Si ; les phases dures contiennent Cr, Fe, Mo et C ; et la porosité est inférieure ou égale à 2,0 %. この耐熱焼結材は、全体組成として、質量%でCr:20~38%、Mo:0.5~3.0%、Si:3.0~7.0%、及びC:0.5~2.5%を含有し、残部がFeおよび不可避不純物からなる組成を有し、母相中に硬質相が分散された組織を有し、前記母相がFeとCrとMoとSiを含み、前記硬質相がCrとFeとMoとCを含み、気孔率が2.0%以下である。
Bibliography:Application Number: WO2018JP11756