IMPROVEMENT OF INTER-LAYER-STABILITY OF CERAMIC MATRIX COMPOSITES

By coating green plies (7', 7'', ...) of a green CMC component (4) with Aluminum (Al) before sintering the plies (7', 7'', ...) together, a good interlayer stability is reached for the CMC component (40). En appliquant un revêtement d'aluminium (l) sur des plis cru...

Full description

Saved in:
Bibliographic Details
Main Authors SADOVOY, Alexandr, HOLLINGSWORTH, Peter Stuart
Format Patent
LanguageEnglish
French
Published 14.06.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:By coating green plies (7', 7'', ...) of a green CMC component (4) with Aluminum (Al) before sintering the plies (7', 7'', ...) together, a good interlayer stability is reached for the CMC component (40). En appliquant un revêtement d'aluminium (l) sur des plis crus (7', 7'', ...) d'un composant CMC cru (4) avant le frittage des plis (7', 7'', ...) ensemble, une bonne stabilité inter-couches est obtenue pour le composant CMC (40).
Bibliography:Application Number: WO2017EP78713