PHENOLIC RESIN TO BE BLENDED WITH RUBBER, RUBBER COMPOSITION, AND TIRE

This phenolic resin to be blended with rubber is characterized in that, regarding a chemical shift measured with 13C-NMR, when the total peak surface area in 110-160 ppm is defined as 100, the total peak surface area in 0 ppm or more but less than 60 ppm is 80-400, while the total peak surface area...

Full description

Saved in:
Bibliographic Details
Main Authors SAIKI, Aya, SASAHARA, Yuichi, KUNIMI, Takao, MATSUO, Shigeaki
Format Patent
LanguageEnglish
French
Japanese
Published 02.11.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:This phenolic resin to be blended with rubber is characterized in that, regarding a chemical shift measured with 13C-NMR, when the total peak surface area in 110-160 ppm is defined as 100, the total peak surface area in 0 ppm or more but less than 60 ppm is 80-400, while the total peak surface area of 60 ppm or more but less than 110 ppm is 2-70. Cette résine phénolique à mélanger avec du caoutchouc est caractérisée en ce que, concernant un décalage chimique mesuré avec la RMN 13C, lorsque la surface de crête totale comprise entre 110 et 160 ppm est définie comme étant égale à 100, la surface de crête totale de 0 ppm ou plus mais inférieure à 60 ppm est de 80 à 400, tandis que la surface de crête totale de 60 ppm ou plus mais inférieure à 110 ppm est de 2-70. 本発明に係るゴム配合用フェノール樹脂は、13C-NMRによる化学シフト、110ppm以上160ppm以下のピーク面積の総和を100としたとき、0ppm以上60ppm未満のピーク面積の総和が80~400であり、60ppm以上110ppm未満のピーク面積の総和が2~70であることを特徴とする。
Bibliography:Application Number: WO2017JP14104