RUBBER-MODIFIED PHASE-CHANGE THERMALLY-CONDUCTIVE INTERFACE MATERIAL AND PREPARATION METHOD
A rubber-modified phase-change thermally-conductive interface material and a preparation method. The phase-change thermally-conductive interface material comprises raw materials in the following weight percentages: 3%-10% of a basic phase-change resin, 1%-5% of a synthetic rubber, 5%-10% of a tackif...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | Chinese English French |
Published |
08.06.2017
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A rubber-modified phase-change thermally-conductive interface material and a preparation method. The phase-change thermally-conductive interface material comprises raw materials in the following weight percentages: 3%-10% of a basic phase-change resin, 1%-5% of a synthetic rubber, 5%-10% of a tackifying resin, 0%-1% of an antioxidant, 0%-5% of a coupling agent and 69%-85% of thermally-conductive particles. The rubber-modified phase-change thermally-conductive interface material has an improved heat conduction performance.
La présente invention concerne un matériau d'interface thermoconducteur à changement de phase modifié par du caoutchouc et un procédé de préparation associé. Le matériau d'interface thermoconducteur à changement de phase comprend des matières premières en les pourcentages en poids suivants : 3 % à 10 % d'une résine à changement de phase basique, 1 % à 5 % d'un caoutchouc synthétique, 5 % à 10 % d'une résine donnant du collant, 0 % à 1 % d'un antioxydant, 0 % à 5 % d'un agent de couplage et 6 |
---|---|
Bibliography: | Application Number: WO2015CN96969 |