METHOD FOR FORMING A LOW VISCOSITY POLYARYLENE SULFIDE

A method for washing a polyarylene sulfide with a washing solution that contains a carefully controlled solvent content is provided. More particularly, the washing solution typically contains water (e.g., deionized water) in an amount of from about 30 wt.% to about 70 wt.% and an aprotic organic sol...

Full description

Saved in:
Bibliographic Details
Main Authors NEKKANTI, Venkata M, CHIONG, Hendrich A, GRAYSON, Jacob
Format Patent
LanguageEnglish
French
Published 25.08.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for washing a polyarylene sulfide with a washing solution that contains a carefully controlled solvent content is provided. More particularly, the washing solution typically contains water (e.g., deionized water) in an amount of from about 30 wt.% to about 70 wt.% and an aprotic organic solvent in an amount of from about 30 wt.% to about 70 wt.%. Within such carefully controlled ranges, the present inventors have discovered that the polyarylene sulfide can retain a relatively high oligomer content, which in turn, helps minimize the melt viscosity. La présente invention concerne un procédé de lavage d'un sulfure de polyarylène avec une solution de lavage dont la teneur en solvant est soigneusement contrôlée. Plus particulièrement, la solution de lavage renferme généralement de l'eau (par exemple, de l'eau désionisée) à hauteur d'environ 30 % en poids à environ 70 % en poids et un solvant organique aprotique à hauteur d'environ 30 % en poids à environ 70 % en poids. À l'intérieur de ces plages soigneusement contrôlées, les présents inventeurs ont découvert que le sulfure de polyarylène peut conserver une teneur en oligomères relativement élevée, qui à son tour, contribue à réduire au minimum la viscosité à l'état fondu.
Bibliography:Application Number: WO2016US17079