RUBBER COMPOSITION

A rubber composition which has both improved wear resistance and improved rolling resistance without deteriorating wet grip performance thereof. The rubber composition comprises: 100 parts by mass of a rubber component containing 30 mass% or more of polyisoprene; and 2 to 200 parts by mass of carbon...

Full description

Saved in:
Bibliographic Details
Main Author AOMATSU KEIICHI
Format Patent
LanguageEnglish
French
Japanese
Published 27.11.2014
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A rubber composition which has both improved wear resistance and improved rolling resistance without deteriorating wet grip performance thereof. The rubber composition comprises: 100 parts by mass of a rubber component containing 30 mass% or more of polyisoprene; and 2 to 200 parts by mass of carbon black which has a hydrogen release rate of 0.2 mass% or more and/or a ratio (N2SA/CTAB) of a nitrogen-adsorbed specific surface area (N2SA) to a cetyltributylammonium-adsorbed specific surface area (CTAB) of 1.2 to 1.5 and also has a nitrogen-adsorbed specific surface area (N2SA) of 160 to 300 m2/g. L'invention porte sur une composition de caoutchouc ayant tant une résistance améliorée à l'usure qu'une résistance améliorée au roulement, sans dégradation de ses performances d'adhérence sur sol mouillé. La composition de caoutchouc comprend : 100 parties en masse d'un composant caoutchouc contenant 30 % en masse ou plus de polyisoprène ; et 2 à 200 parties en masse d'un noir de carbone ayant un taux de dégagement d'hydrogène de 0,2 % en masse ou plus et/ou un rapport (N2SA/CTAB), entre l'aire spécifique à adsorption d'azote (N2SA) et l'aire spécifique à adsorption de cétyltributylammonium (CTAB) de 1,2 à 1,5, et a aussi une aire spécifique mesurée par adsorption d'azote (N2SA) de 160 à 300 m2/g.
Bibliography:Application Number: WO2014JP63562