OPTICAL POLYMER AND OPTICAL ELEMENT OBTAINED BY FORMING THEREOF

An optical polymer which satisfies formula (1) when the melt viscosity at a shear rate of 200 (1/s) at 290°C is A and the melt viscosity at a shear rate of 2000 (1/s) at 290°C is B. ( A- B)/ B×100<60 (1) L'invention porte sur un polymère optique qui satisfait à la formule (1), où A est la vi...

Full description

Saved in:
Bibliographic Details
Main Authors KOMATSUBARA TAKUYA, HARAUCHI YOSUKE, UMEDA KENJI, HOUKAWA TAKASHI, NISHIOKA HIROYA, SATO AYUMI
Format Patent
LanguageEnglish
French
Japanese
Published 03.07.2014
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An optical polymer which satisfies formula (1) when the melt viscosity at a shear rate of 200 (1/s) at 290°C is A and the melt viscosity at a shear rate of 2000 (1/s) at 290°C is B. ( A- B)/ B×100<60 (1) L'invention porte sur un polymère optique qui satisfait à la formule (1), où A est la viscosité à l'état fondu à un taux de cisaillement de 200 (1/s) à 290°C et B est la viscosité à l'état fondu à un taux de cisaillement de 2 000 (1/s) à 290°C : ( A - B)/ B × 100 < 60 (1).