LOW VISCOSITY HIGH SOLIDS COPOLYMER

A copolymer is made by feeding one or more added olefinic monomers into a reaction vessel containing a non-homopolymerizable olefinic monomer heated to a temperature of at least about 100° C. The process may be performed in a batch or continuous fashion, may use an unpressurized reactor, may be perf...

Full description

Saved in:
Bibliographic Details
Main Author CAVALLIN, CARL, LEWIS
Format Patent
LanguageEnglish
French
Published 16.12.2010
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A copolymer is made by feeding one or more added olefinic monomers into a reaction vessel containing a non-homopolymerizable olefinic monomer heated to a temperature of at least about 100° C. The process may be performed in a batch or continuous fashion, may use an unpressurized reactor, may be performed without added solvent, and may form a copolymer whose number average molecular weight is less than about 4,000 amu and whose polydispersity is less than about 3. La présente invention concerne un copolymère fabriqué en introduisant un ou plusieurs monomères oléfiniques supplémentaires dans un réacteur contenant un monomère oléfinique non homopolymérisable chauffé à une température d'au moins environ 100 °C. Le procédé peut être mis en oeuvre de façon continue ou discontinue, peut utiliser un réacteur qui n'est pas sous pression, peut être mis en oeuvre sans solvant ajouté, et peut former un copolymère dont le poids moléculaire moyen en nombre est inférieur à environ 4 000 amu et dont la polydispersité est inférieure à 3.
Bibliography:Application Number: WO2010US38091