Tissue having high strength and low modulus
The present invention provides tissue products having a high degree of stretch and low modulus at relatively high tensile strengths, such as geometric mean tensile strengths greater than about 1500 g/3″ and more preferably greater than about 2000 g/3″. The combination of a tough, yet relatively supp...
Saved in:
Main Authors | , , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
09.08.2016
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The present invention provides tissue products having a high degree of stretch and low modulus at relatively high tensile strengths, such as geometric mean tensile strengths greater than about 1500 g/3″ and more preferably greater than about 2000 g/3″. The combination of a tough, yet relatively supple sheet is preferably achieved by subjecting the embryonic web to a speed differential as it is passed from one fabric in the papermaking process to another, commonly referred to as rush transfer. |
---|---|
Bibliography: | Application Number: US201514932158 |