Automotive interior compound

Composition having a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 15 to 30 g/10 min, said composition comprises a heterophasic propylene copolymer (H-PP1), a high melt flow polypropylene (HMF-PP), a styrenic block copolymer (SBC) and a mineral filler (F), wherein (a)...

Full description

Saved in:
Bibliographic Details
Main Authors KASTNER ERWIN, LEDERER KLAUS
Format Patent
LanguageEnglish
Published 08.12.2015
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Composition having a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 15 to 30 g/10 min, said composition comprises a heterophasic propylene copolymer (H-PP1), a high melt flow polypropylene (HMF-PP), a styrenic block copolymer (SBC) and a mineral filler (F), wherein (a) the heterophasic propylene copolymer (H-PP1) has a xylene cold soluble (XCS) content measured according to ISO 6427 in the range of 22.0 to 50.0 wt.-% and comprises (a1) a polypropylene matrix (M1) and (a2) an elastomeric copolymer (E1) comprising units derived from propylene and ethylene and/or C4 to C12 α-olefin, (b) the melt flow rate MFR2 (230° C.) measured according to ISO 1133 of the high melt flow polypropylene (HMF-PP) is higher than the melt flow rate MFR2 (230° C.) measured according to ISO 1133 of the heterophasic propylene copolymer (H-PP1), and (c) the high melt flow polypropylene (HMF-PP) has melt flow rate MFR2 (230° C.) measured according to ISO 1133 of at least 40.0 g/10 min.
Bibliography:Application Number: US201113639961