Methods of resizing holes
Methods of reducing an initial cross-sectional area of a hole in a component to a predetermined cross-sectional area including preparing a composition comprising at least an aluminum alloy with a melting temperature higher than aluminum, applying the composition to an interior surface of the hole, a...
Saved in:
Main Authors | , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
17.11.2015
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Methods of reducing an initial cross-sectional area of a hole in a component to a predetermined cross-sectional area including preparing a composition comprising at least an aluminum alloy with a melting temperature higher than aluminum, applying the composition to an interior surface of the hole, and then heating the component to cause a metal within the component to diffuse from the component into the composition and react with the aluminum alloy in the composition to form a coating on the interior surface of the hole. The heating step is performed to selectively modify the initial cross-sectional area of the hole and thereby directly attain the predetermined cross-sectional area thereof. |
---|---|
Bibliography: | Application Number: US201213669754 |