Alkenyl aromatic foam with low solubility hydrofluorocarbon
Prepare a closed-cell alkenyl aromatic polymer foam by an extrusion process using a blowing agent composition that contains at least 30 weight-percent of the chlorine-free hydrofluorocarbon blowing agent such that the foam has a density of 48 kilograms per cubic meter or less, contains more than 50...
Saved in:
Main Authors | , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
22.07.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Prepare a closed-cell alkenyl aromatic polymer foam by an extrusion process using a blowing agent composition that contains at least 30 weight-percent of the chlorine-free hydrofluorocarbon blowing agent such that the foam has a density of 48 kilograms per cubic meter or less, contains more than 50 weight-percent styrene-acrylonitrile copolymer based on total polymer weight and at least eight weight-percent of a chlorine-free hydrofluorocarbon blowing agent that has a lower solubility in polystyrene than 1,1,2,2-tetrafluoroethane (HFC-134). |
---|---|
Bibliography: | Application Number: US20080531518 |