Method of producing rolling sliding member

A method of producing a rolling sliding member, wherein, after a work for a rolling sliding member, which is made of a bearing steel and formed in a predetermined shape, is quenched, a heating start temperature is set to be 10 to 100° C., a heating finish temperature is set to be 220 to 350° C., a t...

Full description

Saved in:
Bibliographic Details
Main Authors MATSUI TOWAKO, KIZAWA KATSUHIKO
Format Patent
LanguageEnglish
Published 04.02.2014
Subjects
Online AccessGet full text

Cover

More Information
Summary:A method of producing a rolling sliding member, wherein, after a work for a rolling sliding member, which is made of a bearing steel and formed in a predetermined shape, is quenched, a heating start temperature is set to be 10 to 100° C., a heating finish temperature is set to be 220 to 350° C., a time between the heating finish time and the heating start time is set to be a heating time, the quenched work for the rolling sliding member is heated so that a rate of temperature increase indicated by the following formula becomes 7 to 35° C./s rate of temperature increase=(heating finish temperature-heating start temperature)/heating time, the work is tempered by being cooled without being maintained at a heating finish temperature from the heating finish time.
Bibliography:Application Number: US20100853911