Highly crystalline polypropylene with low xylene solubles
The invention is directed to a polypropylene resin which has a Mw/Mn of less than 5, a melt flow rate of less than 7 g/10 min., a 1% secant flexural modulus of greater than 300,000 psi and less than 2 wt. % xylene solubles.
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
08.08.2006
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention is directed to a polypropylene resin which has a Mw/Mn of less than 5, a melt flow rate of less than 7 g/10 min., a 1% secant flexural modulus of greater than 300,000 psi and less than 2 wt. % xylene solubles. |
---|---|
Bibliography: | Application Number: US20030680372 |