Composition and process for preventing corrosion and reducing friction on metallic surfaces
PCT No. PCT/EP95/04469 Sec. 371 Date May 23, 1997 Sec. 102(e) Date May 23, 1997 PCT Filed Nov. 14, 1995 PCT Pub. No. WO96/16205 PCT Pub. Date May 30, 1996Aqueous acid treatment solution for the treatment of beverage cans, in particular of aluminum, for producing a corrosion-protective, friction-redu...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
10.08.1999
|
Edition | 6 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PCT No. PCT/EP95/04469 Sec. 371 Date May 23, 1997 Sec. 102(e) Date May 23, 1997 PCT Filed Nov. 14, 1995 PCT Pub. No. WO96/16205 PCT Pub. Date May 30, 1996Aqueous acid treatment solution for the treatment of beverage cans, in particular of aluminum, for producing a corrosion-protective, friction-reducing coating which improves the ability to be enameled, which comprises 0.14 to 2.25 mmol/l of an alkylamine oxide or an alkylammonium salt with an alkyl radical having 8 to 22 C atoms, 0.25-1.5 mmol/l of hydroxycarboxylic acids having 4-7 C atoms, complex fluorides and mineral acids, and preferably tannin. |
---|---|
Bibliography: | Application Number: US19970849411 |