Process and gaseous mixture for arc welding of aluminium components
The arc welding, with a refractory electrode, using alternating current, is performed with a gaseous protective mixture including at the location of the weld, at least 50%, typically between 60 and 80% of helium and at least 300 vpm, typically between 400 and 800 vpm, of nitrogen, the remainder bein...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
16.09.1997
|
Edition | 6 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The arc welding, with a refractory electrode, using alternating current, is performed with a gaseous protective mixture including at the location of the weld, at least 50%, typically between 60 and 80% of helium and at least 300 vpm, typically between 400 and 800 vpm, of nitrogen, the remainder being argon. Application to manual or automatic welding of aluminium components. |
---|---|
Bibliography: | Application Number: US19960707615 |