Polyethylene blends
A composition of matter comprising: (a) 5 to 40 weight percent inclusive of a low molecular weight ethylene resin made using a titanium catalyst system said resin having a density greater than 0.955 grams per cubic centimeter, a melt index greater than 25 grams per 10 minutes, and a heterogeneity in...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English |
Published |
07.06.1994
|
Edition | 5 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A composition of matter comprising: (a) 5 to 40 weight percent inclusive of a low molecular weight ethylene resin made using a titanium catalyst system said resin having a density greater than 0.955 grams per cubic centimeter, a melt index greater than 25 grams per 10 minutes, and a heterogeneity index between 2 and 8 inclusive; and (b) 60 to 95 weight percent inclusive of a high molecular weight ethylene copolymer resin made using a chromium catalyst system said resin having a density of at least 0.93 grams per cubic centimeter, a high load melt index between 1.5 and 15 grams per 10 minutes, and a heterogeneity index between 6 and 100 inclusive; wherein said composition of matter has a melt index greater than 0.05 grams per 10 minutes. |
---|---|
Bibliography: | Application Number: US19930048631 |