Toughened mercaptosiloxane modified emulsion polymerized vinylic polymers

The impact strength of certain thermoplastic vinylic polymers is improved by polymerizing the corresponding monomers in an emulsion of a diorganosiloxane containing units of the formula HSR'SiRnO3-n/2. For example a styrene acrylonitrile copolymer containing 20 percent by weight of a dimethylsi...

Full description

Saved in:
Bibliographic Details
Main Authors METTLER; CLAUDIA M, FALENDER; JAMES R, SAAM; JOHN C
Format Patent
LanguageEnglish
Published 31.01.1978
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The impact strength of certain thermoplastic vinylic polymers is improved by polymerizing the corresponding monomers in an emulsion of a diorganosiloxane containing units of the formula HSR'SiRnO3-n/2. For example a styrene acrylonitrile copolymer containing 20 percent by weight of a dimethylsiloxane-3-mercaptopropylsiloxane copolymer having 1 mol percent mercaptosiloxane has an Izod notched impact strength of 10.8 foot pounds per inch.
Bibliography:Application Number: US19760679595