METHOD FOR MANUFACTURING LOW LOSS OPTICAL FIBERS

An optical fiber includes a core region of silica glass doped with an alkali metal oxide. A depressed-index cladding region surrounds the core region and comprises silica glass doped with a first concentration of fluorine. The depressed-index cladding region has a minimum relative refractive index Δ...

Full description

Saved in:
Bibliographic Details
Main Authors Matthews, III, Hazel Benton, Tandon, Pushkar, Khrapko, Rostislav Radiyevich
Format Patent
LanguageEnglish
Published 01.06.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An optical fiber includes a core region of silica glass doped with an alkali metal oxide. A depressed-index cladding region surrounds the core region and comprises silica glass doped with a first concentration of fluorine. The depressed-index cladding region has a minimum relative refractive index Δ3min in a range from −0.80% to −0.30%. An outer cladding region comprises silica glass doped with a second, lesser concentration. The outer cladding region has a relative refractive index Δ4, where Δ4−Δ3min>0.05%. The optical fiber has a time-to-peak hydrogen aging value at 23° C. of less than 100 hours upon exposure to an atmosphere having a total pressure of 1 atm and containing a partial pressure of 0.01 atm H2 and a partial pressure of 0.99 atm N2. The optical fiber exhibits an attenuation <0.16 dB/km.
Bibliography:Application Number: US202217989988