ENVIRONMENTALLY FRIENDLY ANTI-CORROSION COATING MATERIAL AND METHOD FOR PREPARING THE SAME

An environmentally friendly anti-corrosion coating material and a method for preparing the same are provided. The environmentally friendly anti-corrosion coating material includes 80 to 90 parts by weight of an epoxy resin, 3 to 7 parts by weight of at least one conductive polymer, 55 to 65 parts by...

Full description

Saved in:
Bibliographic Details
Main Authors YEN, SHIH-HSUN, TSAO, CHUN, LIAO, TEAO
Format Patent
LanguageEnglish
Published 25.08.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An environmentally friendly anti-corrosion coating material and a method for preparing the same are provided. The environmentally friendly anti-corrosion coating material includes 80 to 90 parts by weight of an epoxy resin, 3 to 7 parts by weight of at least one conductive polymer, 55 to 65 parts by weight of curing agent, and at least one functional additive. The at least one conductive polymer is selected from the group consisting of polyacetylene, polypyrrole, polyaniline, polythiophene and poly(p-phenylene).
Bibliography:Application Number: US202117394411