Summary:The method for producing a pigment-kneaded product includes a step [1] of supplying at least a pigment and a resin to a container provided in a kneading apparatus and a step [2] of kneading the resulting content (content (a1)) present in the container until a storage elastic modulus of content (a1) at an angular frequency of 1 rad/s, which is obtained by measurement of dynamic viscoelasticity at 25° C., reaches a range of 200 kPa to 30,000 kPa.