METHOD FOR PRODUCING ALLOY RIBBON

After an first heat treatment step, an ambient temperature of a stack (10) is held so that the stack (10) is kept in a temperature range that allows the stack (10) to be crystallized by heating the end of the stack (10) to a second temperature range in the second heat treatment step; and a following...

Full description

Saved in:
Bibliographic Details
Main Authors KOMORI, Kensuke, MANABE, Hideki, HIRAMATSU, Shinichi, TAKANEZAWA, Yu, TAKAO, Tomohiro
Format Patent
LanguageEnglish
Published 16.07.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:After an first heat treatment step, an ambient temperature of a stack (10) is held so that the stack (10) is kept in a temperature range that allows the stack (10) to be crystallized by heating the end of the stack (10) to a second temperature range in the second heat treatment step; and a following expression (1) is satisfied, where Q1 represents an amount of heat required to heat the stack (10) to the first temperature range in the first heat treatment step, Q2 represents an amount of heat that is applied to the stack (10) when heating the end of the stack (10) to the second temperature range in the second heat treatment step, Q3 represents an amount of heat that is released during crystallization of the stack (10), and Q4 represents an amount of heat required to heat the entire stack (10) to the crystallization start temperatureQ1+Q2+Q3≥Q4
Bibliography:Application Number: US201916725028