MICROPOWDER AND METHOD FOR MANUFACTURING THE SAME

A method for manufacturing micropowder is provided, which includes (a) mixing a silicon precursor and a carbon precursor to form a mixture, and heating and keeping the mixture at 1600° C. to 1800° C. under a vacuum and non-oxygen condition for 120 to 180 minutes to form a silicon carbide powder; and...

Full description

Saved in:
Bibliographic Details
Main Authors SUNG, Mu-Hsi, HSIAO, Ta-Ching, TU, Wen-Po, JENG, Chu-Pi
Format Patent
LanguageEnglish
Published 17.05.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for manufacturing micropowder is provided, which includes (a) mixing a silicon precursor and a carbon precursor to form a mixture, and heating and keeping the mixture at 1600° C. to 1800° C. under a vacuum and non-oxygen condition for 120 to 180 minutes to form a silicon carbide powder; and (b) heating and keeping the silicon carbide powder at 1900° C. to 2100° C. under non-oxygen condition for 5 to 15 minutes, and then cooling and keeping the silicon carbide powder at 1800° C. to 2000° C. under the non-oxygen condition for 5 to 15 minutes to form micropowder, wherein the micropowder includes a silicon carbide core covered by a carbon film.
Bibliography:Application Number: US201615386749