INORGANIC PARTICULATE SUSPENSION HAVING IMPROVED HIGH SHEAR VISCOSITY

An inorganic particulate suspension may include a first kaolin having a shape factor of at least about 70, and a second kaolin having a shape factor less than or equal to about 20. The first kaolin and the second kaolin form a kaolin composition, which may have a content ratio of the first kaolin to...

Full description

Saved in:
Bibliographic Details
Main Authors PANFIL Daniel J, WYGANT Roger, JONES Phil, BOOTHBY Christ, LYONS Anthony V
Format Patent
LanguageEnglish
Published 15.12.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An inorganic particulate suspension may include a first kaolin having a shape factor of at least about 70, and a second kaolin having a shape factor less than or equal to about 20. The first kaolin and the second kaolin form a kaolin composition, which may have a content ratio of the first kaolin to the second kaolin ranging from about 90:10 to about 50:50. An inorganic particulate suspension may include a kaolin composition having a shape factor ranging from about 55 to about 75, wherein at least about 70% to about 90% by weight of the particles of the kaolin composition have an equivalent spherical diameter less than 2 microns. The suspension may have a Hercules viscosity ranging from about 600 rpm to about 700 rpm at 18.0 dyne using an "A" bob, and the suspension may have a solids content ranging from about 55% to about 75% solids.
Bibliography:Application Number: US201515121639