CATHODE ACTIVE MATERIAL AND METHOD FOR MAKING THE SAME
A method for making a cathode active material of a lithium ion battery, the cathode active material being represented by a chemical formula of Li[(Ni0.8Co0.1Mn0.1)1-xMox]O2, wherein 0<x≦0.05. Source liquid solutions of Li, Ni2+, Co2+, Mn2+, and Mo6+ are mixed in stoichiometric ratio in a multi-ca...
Saved in:
Main Authors | , , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
11.08.2016
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A method for making a cathode active material of a lithium ion battery, the cathode active material being represented by a chemical formula of Li[(Ni0.8Co0.1Mn0.1)1-xMox]O2, wherein 0<x≦0.05. Source liquid solutions of Li, Ni2+, Co2+, Mn2+, and Mo6+ are mixed in stoichiometric ratio in a multi-carboxylic acid solution to form a solution. The solution is heated at 50° C. to 80° C. to form a wet gel. The wet gel is spray dried to form a dry gel. The dry gel is heated at a first temperature and then at a second temperature, the first temperature is in a range of 400° C. to 500° C., the second temperature is in a range of 750° C. to 850° C. |
---|---|
Bibliography: | Application Number: US201615099504 |