Internal Mechanical Stress Improvement Method for Mitigating Stress Corrosion Cracking in Weld Areas of Nuclear Power Plant Piping

Method for mitigating stress corrosion cracking at an internal (i.e., welled-side) weld area in piping of a nuclear power plant includes the steps of actuating a radially movable tool to produce a radial bad against the internal (i.e., normally wetted) surfaces at or near the weld area to create a d...

Full description

Saved in:
Bibliographic Details
Main Authors RACKIEWICZ DAVID W, KEPPLE ALAN C, NESTELL JAMES E
Format Patent
LanguageEnglish
Published 04.02.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Method for mitigating stress corrosion cracking at an internal (i.e., welled-side) weld area in piping of a nuclear power plant includes the steps of actuating a radially movable tool to produce a radial bad against the internal (i.e., normally wetted) surfaces at or near the weld area to create a deep residual compressive stress state at the wetted surface of the weld. The method permits post-process verification by physical measurements of surface distortion.
Bibliography:Application Number: US201514622431