FERRITE SINTERED BODY AND MANUFACTURING METHOD THEREFOR
The ferrite sintered body of the present invention contains main components consisting of 52 to 54 mol % Fe2O3, 35 to 42 mol % MnO and 6 to 11 mol % ZnO as oxide equivalents and additives including Co, Ti, Si and Ca in specified amounts, and has a temperature at which the power loss is a minimal val...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
01.10.2009
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The ferrite sintered body of the present invention contains main components consisting of 52 to 54 mol % Fe2O3, 35 to 42 mol % MnO and 6 to 11 mol % ZnO as oxide equivalents and additives including Co, Ti, Si and Ca in specified amounts, and has a temperature at which the power loss is a minimal value (bottom temperature) of higher than 120° C. in a magnetic field with an excitation magnetic flux density of 200 mT and a frequency of 100 kHz, and a power loss of 350 kW/m3 or less at the bottom temperature. |
---|---|
Bibliography: | Application Number: US20090408842 |