New and novel engineering resin thermoplastic silicone vulcanizates

A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a tg of 95° C. or greater and having a melt processing temperature of 250° C. or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an average of at least...

Full description

Saved in:
Bibliographic Details
Main Authors MEHTA VEERAG YAGNIK, ROMENESKO DAVID
Format Patent
LanguageEnglish
Published 07.05.2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a tg of 95° C. or greater and having a melt processing temperature of 250° C. or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an average of at least 2 alkenyl groups per molecule in conjunction with 0 to 50 parts by weight of a reinforcing filler along with a radical initiator. The silicone base and this combination are dynamically vulcanized to cure the silicone base at an elevated temperature.
Bibliography:Application Number: US20070982047