Process for manufacturing glass optical elements
Disclosed are processes for manufacturing glass optical elements by press molding a heated and softened glass material in preheated molds. In the process, the glass material is heated while it is floated by a gas blow and the heated and softened glass material is transferred to the preheated molds a...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English |
Published |
21.08.2003
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Disclosed are processes for manufacturing glass optical elements by press molding a heated and softened glass material in preheated molds. In the process, the glass material is heated while it is floated by a gas blow and the heated and softened glass material is transferred to the preheated molds and then subjected to press molding. Alternatively, the process comprises: heating a glass material at a temperature at which the glass material has a viscosity of lower than 109 poises, preheating molds at a temperature at which the glass material has a viscosity of from 109 to 1012 poises, subjecting the heated and softened glass material to initial press in the preheated molds for 3 to 60 seconds, starting to cool the vicinity of molding surfaces of the molds at a rate of 20° C./minute or higher upon starting of, or during, or after the initial press, and removing a molded glass article from the molds after the temperature of the vicinity of the molding surfaces of the molds becomes a temperature equal to or lower than a temperature at which the glass material has a viscosity of 1012 poises. |
---|---|
Bibliography: | Application Number: US20020309283 |