Conversion of CO TO CO2
Gold oxide is precipitated together with iron oxide from a solution containing a gold source and an iron source; the gel formed thereby is washed, dried, ground to a size range of 0.85 mm to 4.25 mm and calcined; then used as a catalyst for oxidizing CO to CO2 in the presence of a large excess of hy...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English |
Published |
29.05.2003
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Gold oxide is precipitated together with iron oxide from a solution containing a gold source and an iron source; the gel formed thereby is washed, dried, ground to a size range of 0.85 mm to 4.25 mm and calcined; then used as a catalyst for oxidizing CO to CO2 in the presence of a large excess of hydrogen. |
---|---|
Bibliography: | Application Number: US20010997617 |