High voltage, low pressure plasma enhanced atomic layer deposition

Atomic layer deposition (ALD) methods and barrier films are disclosed. A method of performing ALD includes placing a substrate proximal an electrode coupled to a power supply, exposing the substrate to an oxygen-containing gas or a nitrogen-containing gas at or below 0.8 Torr, and applying, with the...

Full description

Saved in:
Bibliographic Details
Main Author Dickey, Eric R
Format Patent
LanguageEnglish
Published 19.03.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Atomic layer deposition (ALD) methods and barrier films are disclosed. A method of performing ALD includes placing a substrate proximal an electrode coupled to a power supply, exposing the substrate to an oxygen-containing gas or a nitrogen-containing gas at or below 0.8 Torr, and applying, with the power supply, a voltage to the electrode of at least 700 Volts to induce a plasma state in the oxygen-containing gas or the nitrogen-containing gas proximal the substrate. High quality barrier films can be made with the methods.
Bibliography:Application Number: US202016866497