Rubber composition for stiffness
A rubber composition for incorporation in an engineered article comprises, based on 100 parts by weight (phr) ethylene-propylene-diene copolymer (EPDM) elastomer, from about 5 phr to about 100 phr reinforcing filler preferably comprising a prehydrophobated precipitated silica. In the contemplated em...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English |
Published |
26.12.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A rubber composition for incorporation in an engineered article comprises, based on 100 parts by weight (phr) ethylene-propylene-diene copolymer (EPDM) elastomer, from about 5 phr to about 100 phr reinforcing filler preferably comprising a prehydrophobated precipitated silica. In the contemplated embodiment, the EPDM has a diene content that is greater than five percent (5%). The diene also contains branching. |
---|---|
Bibliography: | Application Number: US202217656012 |