Elastomeric article

An elastomeric formulation comprising elastomers, accelerator, antifoaming agent, antioxidant, crosslinker, colouring agent, surfactant, filler, pH adjuster and dispersing medium, wherein the elastomeric formulation has a total solid content ranging between 5% by weight to 40% by weight. Further, th...

Full description

Saved in:
Bibliographic Details
Main Authors Lim, Keuw Wei, Wong, Chong Ban, Mok, Chun Fah, Teh, Chee Yang
Format Patent
LanguageEnglish
Published 06.06.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An elastomeric formulation comprising elastomers, accelerator, antifoaming agent, antioxidant, crosslinker, colouring agent, surfactant, filler, pH adjuster and dispersing medium, wherein the elastomeric formulation has a total solid content ranging between 5% by weight to 40% by weight. Further, the present invention discloses a method of preparing an elastomeric formulation to manufacture hybrid elastomeric glove, wherein the method comprises the steps of blending Elastomer A with Elastomer B to produce hybrid elastomer and stirring the hybrid elastomer, adding while stirring accelerator, antifoaming agent, antioxidant, crosslinker, colouring agent, surfactant and filler one after another with no particular order and followed by pH adjuster into the hybrid elastomer to produce elastomeric formulation and stirring the elastomeric formulation continuously and allowing the elastomeric formulation to mature, wherein total solid content of the elastomeric formulation is adjusted to be between 5% by weight to 40% by weight by way of addition of dispersing medium into the elastomeric formulation and wherein pH range of the elastomeric formulation is adjusted to be between 9 to 11.
Bibliography:Application Number: US202017035506