Nucleated C3C4 copolymers
A propylene copolymer composition comprising A) a propylene butylene copolymer which is-free of phthalicacid esters as well as decomposition products thereof; -obtained by a Ziegler-Natta catalyst and B) at least one α-nucleating agent, the propylene copolymer composition having-a MFR (2.16 kg/210°...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English |
Published |
01.02.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A propylene copolymer composition comprising A) a propylene butylene copolymer which is-free of phthalicacid esters as well as decomposition products thereof; -obtained by a Ziegler-Natta catalyst and B) at least one α-nucleating agent, the propylene copolymer composition having-a MFR (2.16 kg/210° C.) in the range of 2 to 100 g/10 min-a melting point Tm(1) of less than 140° C.-a melting point Tm(2) of at least 150° C., said Tm(2) being associated with more than 75% of the total melting enthalpy and whereby the propylene copolymer-has monomer units derived from a) propylene in an amount of 90.0-98.0 mol.-% b) butylene in an amount of 2.0-10.0 mol.-% with respect to the total weight of the propylene butylene copolymer-an isotacticity mm % as determined by 13C NMR spectroscopy of below 99.0%; and-a Koenig-B parameter with respect to butylene as determined by 13C NMR spectroscopy of more than 0.98. |
---|---|
Bibliography: | Application Number: US201816753218 |