Rotomolding processes for poly(aryl ketones) and other high temperature polymers

A method of manufacturing an article comprises rotomolding at least one polymer comprising a poly(aryl ketone), such as PEKK, under conditions effective to produce a rotomolded article having an impact value of at least 35 in-lbs. A rotomolding method comprises heating the mold for a period of time...

Full description

Saved in:
Bibliographic Details
Main Authors Clay, Bruce, Garcia-Leiner, Manuel A
Format Patent
LanguageEnglish
Published 26.01.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method of manufacturing an article comprises rotomolding at least one polymer comprising a poly(aryl ketone), such as PEKK, under conditions effective to produce a rotomolded article having an impact value of at least 35 in-lbs. A rotomolding method comprises heating the mold for a period of time after the internal air temperature of the mold reaches the highest melting point of the at least one polymer. Methods also include using a PEKK powder with a bulk density of at least about 400 g/L. Rotomolded articles of the present invention have impact values of between about 40 in-lbs to about 95 in-lbs, and in particular embodiments greater than about 95 in-lbs.
Bibliography:Application Number: US201314387569