Preparation of ultra high molecular weight polyethylene
Particulate ultra high molecular weight polyethylene (pUHMWPE) are disclosed having an intrinsic viscosity (IV) of at least 4 dl/g, a molecular weight distribution Mw/Mn of less than 4.0, a median particle size D50 of between 50 and 200 μm, a residual Ti-content of less than 10 ppm, a residual Si-co...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
12.05.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Particulate ultra high molecular weight polyethylene (pUHMWPE) are disclosed having an intrinsic viscosity (IV) of at least 4 dl/g, a molecular weight distribution Mw/Mn of less than 4.0, a median particle size D50 of between 50 and 200 μm, a residual Ti-content of less than 10 ppm, a residual Si-content of less than 50 ppm, and a total ash content of less than 1000 ppm. |
---|---|