Heat resistant spheroidal graphite cast iron, method of manufacturing the same and engine exhaust system part including the same

Heat resistant spheroidal graphite cast iron having an improved high temperature tensile strength includes carbon (C) in a range of 3.2-3.4 wt %, silicon (Si) in a range of 4.3-4.8 wt %, manganese (Mn) in a range of 0.2-0.3 wt %, molybdenum (Mo) in a range of 0.8-1.0 wt %, vanadium (V) in a range of...

Full description

Saved in:
Bibliographic Details
Main Authors Shim, Dong-Seob, Yang, Sik, Ju, Young-Kyu, Chung, Jong-Kwon, Hwang, Jae-Hyoung, Kim, Sang-Beom, Jung, Ki-Hwan
Format Patent
LanguageEnglish
Published 21.05.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Heat resistant spheroidal graphite cast iron having an improved high temperature tensile strength includes carbon (C) in a range of 3.2-3.4 wt %, silicon (Si) in a range of 4.3-4.8 wt %, manganese (Mn) in a range of 0.2-0.3 wt %, molybdenum (Mo) in a range of 0.8-1.0 wt %, vanadium (V) in a range of 0.4-0.6 wt %, chrome (Cr) in a range of 0.2-0.4 wt %, niobium (Nb) in a range of 0.2-0.4 wt %, inevitable impurities, and a remainder of iron (Fe) based on a total weight of the heat resistant spheroidal graphite cast iron. The heat resistant spheroidal graphite cast iron further includes barium (Ba) in a range of 0.0045-0.0075 wt %. A content ratio of chrome (Cr) and barium (Ba) (Cr/Ba) is in a range from about 26 to about 89.